GP, GL or GH Steel Grit: How to Choose and Test a Hardness Class
Choose GP, GL or GH steel grit by cutting action, machine limits and the required surface finish, then validate the grade with a controlled production trial.
Review the information on this page and confirm product selection against the operating context.
Use GP for routine cleaning and descaling when a wheel-blast process meets its surface requirement with a grit that rounds during circulation. Move to a GL trial when that process needs stronger, more persistent cutting action and the machine permits the higher hardness. Use GH in compatible compressed-air equipment when retaining angular cutting edges is central to the required finish.
The selection turns on three questions: what must the surface achieve, what media can the machine run, and does the grade maintain the result after recycling? Answer them in that order before changing the recurring abrasive specification.
GP, GL and GH: hardness and working behaviour
YUXIN cast steel grit is available in three hardness classes:
Class | Hardness | Behaviour during circulation | Selection priority |
|---|---|---|---|
GP | 42–50 HRC | Becomes progressively more rounded | General cleaning and descaling where the circulating mix delivers the required finish |
GL | 56–60 HRC | Retains cutting edges longer than GP, then loses sharpness during use | Stronger cutting and profiling where GP no longer sustains the required result |
GH | 63–66 HRC | Retains an angular cutting shape | Etching and profiling in equipment designed for hard angular media, particularly compressed-air systems |
The important distinction is the particle shape reaching the workpiece after repeated impacts. A freshly charged GP mix and a circulated GP mix do not have identical cutting characteristics; assess the finish after recycling as well as at the initial charge.
Hardness describes resistance to permanent deformation. Impact durability is a separate question: a sharp particle can still fracture, become undersized and leave the system. Record particle shape, size distribution and material loss together when comparing grades. Ervin's working-mix explanation describes how breakdown, removal of spent fines and fresh additions continually change the circulating population.
Match the class to the machine
Wheel blasting
Check the wheel machine's permitted abrasive type, hardness and size before introducing GL or GH. The wheel, control cage, liners and recovery system must accommodate the chosen media; a better surface finish does not justify operating outside those limits.
A wheel machine running GP is not automatically suitable for GL. Compare the trial grade's hardness and size with the approved media range. If GL is outside that range or the documentation leaves it unresolved, obtain the machine maker's technical approval before charging the system.
GH needs specific approval for wheel use. FerroECOBlast's equipment guidance places GH primarily in compressed-air blasting and identifies specialised wheel applications. Treat a wheel installation approved for GH as a defined equipment/process combination, not permission to use GH in another machine.
Compressed-air blasting
Use GH where the surface task requires sustained angular cutting, then choose the size and process settings to reach the coating's profile range. Include GL in the comparison when it can meet the same surface requirement with a better measured balance of cleaning time, abrasive use and equipment cost.
Record nozzle condition, pressure at the designated measurement point, abrasive feed, angle, stand-off distance and exposure time. Hold these steady for the class comparison. Changing the nozzle or increasing pressure while changing grit makes it impossible to assign the result to hardness alone.
Make the selection from the actual surface problem
The GP wheel process already passes cleanliness and profile
Retain it as the reference process. A change of class needs a measurable objective, such as reducing rework or lowering cost per accepted component. Compare the proposed grade against that objective while preserving the surface result.
If the new grade produces the same finish with no measured operational benefit, keep GP. A higher hardness adds no value to a requirement the existing process already meets.
GP removes scale, but the profile falls below the required range during circulation
First verify the profile measurement, then compare the working mix with the last acceptable run. Check the sieve distribution, recent top-ups, sample location, workpiece condition and machine settings. Restore any changed process condition before treating hardness as the cause.
If these conditions are stable, trial GL at the same specified size in a machine approved for it. Its greater edge retention addresses the cutting-action question directly. Measure the initial result and the result after recycling. Accept the change only if GL sustains both cleanliness and profile without exceeding the machine's operating limits or the agreed wear/cost criteria.
The air-blast surface passes, but dust and abrasive additions rise
Investigate the loss before changing class. Dust comes from the abrasive and from material removed from the workpiece, as explained in Ervin's air-blasting bulletin.
Compare workpiece condition, cleaned feed, recovered media and separator discharge. Look for changed coating/scale load, increased fragmentation, usable grit in the reject stream, leakage and extraction faults. Have maintenance inspect the system using its isolation procedure.
If the evidence points to abrasive breakdown, retain the sample and lot identity for hardness, grading and durability assessment. If usable grit is being discarded, correct the recovery fault first. Increasing hardness will not recover abrasive lost through a leak or an incorrectly operating separator.
Validate the grade through a controlled trial
Set cleanliness, profile, component-damage and equipment limits before the trial. Use representative workpieces, including the features most difficult to clean. For general trial planning, see the abrasive selection guide.
Trial stage | Required record | Decision it supports |
|---|---|---|
Baseline | Existing class, grading, working-mix sample, settings, cleanliness, profile, cycle time and rework | Defines the performance the new grade must retain or improve |
Material comparison | New grade's hardness and sieve report; machine approval; unchanged process settings | Identifies the intended class change and any additional material differences |
Changeover | Retained old abrasive, fresh additions and the point at which samples were taken | Separates a mixed-charge transition from operation with the trial grade |
Recycled operation | Same sampling point and method; repeat surface inspections over the agreed trial interval | Shows whether the finish persists as the working mix develops |
Operating result | Accepted output, rework, additions, inventory changes, waste and equipment observations | Compares the surface result and operating burden on the same basis |
Use these decisions at the end of each trial stage:
Hold an area that fails cleanliness, profile or component-damage limits. Hold the process if equipment limits are exceeded.
Repeat a comparison whose settings, workpiece condition or mix composition changed enough to conceal the class effect.
Extend monitoring when the surface passes but the interval is too short to assess additions or equipment wear.
Approve the grade when it meets the full requirement and delivers the improvement defined before the trial.
Measure cleanliness and profile separately. Faster scale removal with excessive profile is a failed surface result. Use the required measurement method, such as the replica-tape method in ISO 8503-5, and apply the coating system's specified range.
Calculate operating cost per accepted component or accepted area using abrasive use, energy, labour, maintenance and waste costs for the same interval. Include rework and account for inventory changes. Record short-trial wear observations as observations; establish a component-life trend over a sufficient operating period before using it in a savings calculation.
Specify the grade that passed
Keep hardness class and size as separate order fields. GP40 and GH40 distinguish the class while retaining the G40 designation. G40 specifies grading rather than a single particle diameter; the shot and grit size guide explains the corresponding specification record.
The recurring order should retain the approved class and hardness range, size specification and edition, lot evidence, trial reference and machine/process condition. A supplier, class or grading change should trigger the site's defined review of whether another trial is required.
Where the contract specifies ISO 11124-3, apply it to incoming high-carbon cast-steel shot or grit. Control the in-use working mix through the approved production sampling and inspection plan.
Request a quote with the established class, size and inspection requirements. For a grade-selection discussion, send the machine's permitted media range and the measured surface problem so the trial can address a defined operating requirement.